When
discussing XPS imaging, the question to answer is why XPS image data does not
appear more in the literature? One reason typically quoted is the lack of
spatial resolution compared to other techniques such as Auger or ToF SIMS;
however this in itself is not sufficient to explain the lack of published data.
The problem with XPS imaging relates to the nature of XPS spectra, where the
signal often sits on the back of broad energy loss features, thus a single
image represents the combined influence of the transition monitored and all
peaks to higher kinetic energy contributing to the background shape. Traditionally,
XPS imaging of a surface consisted of choosing a binding energy representing a
transition from the element of interest, acquiring an image then taking a
second image at an energy representative of the background signal for the
photoelectron peak previously measured. Once the peak and background images are
available, interpretation of the results is based on the difference in counts
per second between the peak and the background images. The rationale behind the
calculation is to extract the signal representative of the peak above the
background; however in spectroscopic terms, these calculations represent a very
primitive mechanism for measuring a photoelectric line. Few analysts today
would quantify XPS spectra using quantities analogous to those used for XPS
imaging. Further, the images typically
include artefacts attributable to the X-ray source, the lens system, the
detection system and sample topography. Thus, visual inspection of individual background
subtracted elemental images is often misleading and so explains why images are
used to guide spectroscopy suitable for publication, but tends not to be seen
as publishable in its own right.
All the
same issues of X-ray flux, lens systems, detection systems and sample
topography also exist for spectroscopy. The issues associated with XPS imaging
then leads to a further question: what is it about spectroscopy that makes the
results acceptable? The solution adopted for spectroscopy is to generate a
normalised quantification report relative to the total composition of the
surface. That is, the measured intensities are corrected for relative
sensitivity and instrumental transmission, summed to provide the normalisation
factor and reported as a set of intensities relative to this normalisation
factor. The resulting percentage atomic concentration report provides a set of
numbers by which different samples can be compared. The introduction of
parallel acquisition, either in terms of energy or spatial dimensions, means
that so called spectromicroscopy where images are
acquired in such a way that spectra at each pixel are available for analysis,
provides the image data in such a fashion that the tried and accepted spectral
analysis techniques can be used to create chemical state image. What is more,
these images generated from spectra at pixels can be interpreted with all the
certainty of normal spectroscopy.
The key to
the success of spectromicroscopy are data consisting
of acceptable signal to noise. Large area analysis achieves good
signal-to-noise by collecting a single spectrum from a relatively large area,
whereas a set of images may be measured from the same area and rather than
summing the signal, counts are assigned to spatially resolved pixels at a given
energy. If a spectrum of images is acquired, it is not surprising to observe
that the spectra at pixels have poor signal-to-noise compared to a single large
area spectrum. Fortunately, multivariate statistics offers a means of analysing
an image dataset into useful information and noise.
The
following discussion is a practical example of spectromicroscopy,
where chemical state images are prepared from spectra at pixel data sets. A
methodology for creating peak models and applying these models to individual
pixel spectra is developed.
A sample
consisting of silicon dioxide islands on elemental silicon provides a good
example of how energy resolved images can be treated using a combination of
Principal Component Analysis (PCA), false colour image partitioning, and
standard spectroscopic techniques to reveal an enhanced understanding for the
nature of the surface.
The image
in Figure 1 represents an example from a set of forty nine images acquired
using a 0.25 eV step-size from 536 to 524 binding
energy at pass energy 80 through a mirror hemi-spherical analyser onto a delay
line image detector (Kratos Axis Ultra at University of Manchester). The
surface was irradiated using an Al monochromatic X-ray source. The XPS image
illustrates some of the issues with the technique, namely, the intensity varies
from bottom left to top right and striations associated with the detection
system are clearly visible.

Figure 1
The set of
images from which the data in Figure 1 was taken also illustrates the
difficulty of selecting a binding energy to represent a specific chemical
state. On summing the pixels in each image and presenting these intensities as
a spectrum (Figure 2), it becomes clear that the various oxide states are
present but form a single peak structure deriving from overlapping component
peaks. The O 1s peak in Figure 2 represents a target for peak modelling, since
the sum of all the pixels necessarily include contributions from all oxygen
states regardless of their spatial separation.

Figure 2
An advantage of spectromicroscopy
is the possibility of isolating information in the spatial domain, and then
generating spectra based on the spatial filter analogously to the spectrum in
Figure 2. If chemically distinct spatial regions exist on the sample, the
possibility of identifying and generating spectra representative of the
components comprising the spectrum in Figure 2 is achievable. The current
example demonstrates how these spectra from sets of similar pixel intensities
can be used to create the peak model for identifying the chemical states on the
surface. Indeed, the
requirement that both the peak model makes chemical sense and the resulting images
are similarly plausible enhances the comfort-factor when interpreting the data
set.
The first task is to prepare an image from which spatial zones can be identified (Figure 3). The false colour image group pixels together based on intensity and therefore if an appropriate image is used to define the false colours, the raw spectra at each pixel can be summed to produce spectra representative of sample chemistry. Figure 4 are the set of spectra generated by summing the coloured zones from the false colour image in Figure 3. A single peak model must be prepared and applied to each of the spectra corresponding to the false colour image; then together the false colour image and these sum-of-colour spectra are used to guide the fitting of the peak model against all the spectra at pixels in the entire O 1s data set. Before fitting the peak model, the PCA based procedure is first applied to the spectra at pixels to produce reduced-noise data.

Figure 3: False colour image corresponding to spectra in Figure 4.
The spectra in Figure 4 are colour coded to match the colours in the false colour image in Figure 3. Each spectrum in Figure 4 includes a four component peak model; the number of components defined for each spectrum must be the same, however, the constraints are at liberty to be adjusted on a spectrum-by-spectrum basis. Similarly, the number of regions defined on the spectra must be the same for each spectrum; however the regions parameters, eg background type, can vary between spectra.

Figure 4: Spectra generated from the false colour image in Figure 3.
The peak models in Figure 4 contain four O 1s synthetic components.
When these peak models are applied to the O 1s data set, where each
spectrum-at-a-pixel is associated with one of these peak models using the false
colour image, the four images in Figure 5 result.
These raw O 1s component images in turn are combined with similarly created
images from the Si 2p data set to produce the
quantified images in Figure 6. The consequence of applying the quantification
transformation is a set of images in which the artifacts due to the
instrumentation are greatly reduced and the chemical state information becomes
more apparent.

Figure 5: Raw O 1s component images.
The beauty of spectromicroscopy is
that the results must be self consistent. That is, a peak model must satisfy
the chemical requirements for the surface and, just as importantly, the images
must make visual sense of the chemistry too. In this particular example, four
peaks where used to analyze the O 1s peaks, where as only two oxide peaks where
extracted from the Si 2p data. The O 1s peaks in
Figure 4 support the need for four synthetic components and so too do the
images in Figure 6. A poorly define peak model could easily result in well
fitted spectra but images at odds with the spatial variation of the surface. In
the current example, the images created from the Si
2p data are similar to the images synthesized from the O 1s data. The remaining
question left unanswered is how these four components within the O 1s image
should be interpreted.

Figure 6: O 1s and Si 2p images following quantification transformation.
The sequence of steps when performing a chemical state analysis of an image data set is as follows.
Some of these steps require further explanation.

Figure 7: Image Processing property page
An appropriate image for creating false colour zones is an image for which the intensities are uniform across the image and the intensity variation is somewhat representative of the chemical states of interest. These requirements may seem to be putting the cart before the horse, however what is required is essentially a first order approximation to the desired chemical state information, not the end result itself. For example, the image used to define the false colour scale in Figure 3 was constructed using two images from the original set of O 1s, one representative of the air-formed oxide and one from the SiO2 islands. The two images were overlaid in the active tile and the Quantify button pressed. The resulting images are I1 / (I1 + I2) and I2 / (I1 + I2) which effectively normalizes the images. Another possible image source might be to use the abstract factors from a PCA.
Once each pixel in an image is assigned a false colour, the template image for summing of pixel spectra into individual spectra is defined using the button labeled Define Image. A buffer is loaded with the false colour image information, which can be used by selecting an Experiment Frame containing the raw spectra-at-pixels data, then pressing the Sum Spectra Using Colours button. The spectra-at-pixels must be created from an image data set for which there is an identical number of rows and columns of pixels to the template image. This statement means there must be no additional VAMAS blocks from those originally created when the images where transformed into spectra at pixels.
Having prepared the spectra at pixels Experiment Frame,
defined the false colour image template and
established a peak model for each of the false colour
spectra, the next step is to press the Convert
Components to Images button. A dialog window (Figure 8) reports the number
of spectral blocks and offers a tick box. The tick box allows the decision
between using the false colour spectra to provide the
source for the peak-model or a peak model taken from the target
spectra-at-pixels. If the tick-box is ticked, then the false colour image guides the peak fit by applying the peak-model
from the false colour spectrum matching the given
pixel colour to each spectrum at a pixel. Once a spectrum-at-pixel
is fitting with a model, the component intensities are extracted and entered
into new images.

Figure 8